Colour, gloss and texture: how we hit a target

The numbers behind a cosmetic approval — what we measure, with which instrument, and what counts as a pass. Bring your own criteria and we will quote against them.

The measurement sheet

What gets measured, and against what

Every cosmetic batch is released against this sheet. If your drawing carries a tighter callout, it replaces the default.

PropertyInstrumentDefault pass criterionTighter option
Colour differenceSpectrophotometer, D65 / 10°ΔE*ab ≤ 1.5 vs approved plaqueΔE ≤ 1.0 on request
Gloss levelGloss meter, 60° geometry± 5 GU of target± 3 GU on flat faces
TextureComparator plaque (SPI / VDI)Visual match at 300 mmComparator match at 150 mm
Clear light transmissionSpectrophotometer, 2 mm section≥ 88% at 550 nm≥ 90%, haze ≤ 2%
Yellowing after ageing72 h QUV, Δb*Δb ≤ 2.0Δb ≤ 1.0 with UV stabiliser
Parting line visibilityVisual under D65 at 400 mmNot visible on A-surfacePolished blend, no witness line
DimensionalCMM / caliper per drawing±0.15 mm / 100 mm±0.05 mm on small parts

Colour

Tinted in the resin, or painted after?

Both work, and they fail differently. Tinting the PU gives depth and hides scratches, but a tint shift is expensive to correct mid-batch. Painting gives an exact Pantone match and lets you change shade at 20 pieces, but it adds a film thickness that shows on tight radii.

  • Resin tinting: best for deep colours, translucent parts and moulded-in look
  • Painting: best for exact brand matches, metallics and 2K soft-touch
  • We spray a plaque in the chosen route and measure it before the run
  • Pantone, RAL and NCS references all accepted; a physical chip is better than a code
Matte champagne cast cap and collar

Gloss and texture

Three ways to get a surface, three different costs

01

Mould-cut texture

Etched into the master before the silicone is poured. Cheapest per part, repeats exactly across the batch, and dies with the mould at 15–25 shots.

02

Spray texture

Applied after casting. Lets you vary the grain per order without a new master, but adds a film that softens sharp edges and can chip on impact.

03

As-printed

MJF gives a fine even grain straight out of the build; SLS reads slightly rougher. Both are honest engineering finishes and cost nothing extra.

LookGloss at 60°Typical routeWears how
Dead matte2–6 GUMatting agent in 2K paintPolishes to sheen where handled
Soft-touch3–8 GUElastomer coatingSkins over years; not for abrasion points
Satin20–30 GUMould-cut VDI 27–30Stable, hides fingerprints
Semi-gloss50–60 GUPaint over polished masterShows wear on high-touch faces
High gloss85+ GUPolished master, clear coatMicro-scratches accumulate visibly

Clear parts

Water-clear is a separate discipline

Clear PU yellows, and it yellows unevenly — thick sections go first. For lenses and light pipes we specify a UV-stabilised grade, cast under vacuum to pull the bubbles, and measure transmission at the thinnest and thickest section of the same part.

If the part has to pass light rather than just look clear, send the photometric requirement with the drawing. It changes the resin choice, not the mould.

Batch of cast PU parts on a steel tray

Questions

Asked before the first batch

Can you match a Pantone colour exactly?

We match the chip, not the code — screen renderings of a Pantone number differ between suppliers. We spray a plaque, measure it under D65 and send the ΔE reading for approval before the batch. Typical result is ΔE ≤ 1.5, and ΔE ≤ 1.0 on flat faces when you specify it.

Will batch two match batch one?

Yes, if we keep the approved plaque and the resin lot records, which we do for repeat parts. Between batches the risk is pigment dispersion in a new resin lot, so we re-measure the first shot of every re-run against the retained plaque rather than against a number.

Can you copy a texture I already mould in steel?

Send a sample or name the SPI or VDI grade. A mould-cut texture is etched into the master and then transferred by the silicone, so it repeats exactly for the life of the tool; a spray texture is applied after casting and is better when you want to vary the grain per order.

Why does a clear part turn yellow after a few months?

Standard clear PU oxidises under UV and the thickest section yellows first. We use a UV-stabilised grade for lenses and light pipes, cast under vacuum to remove bubbles, and quote a Δb limit after 72 hours of QUV so the ageing behaviour is a spec rather than a surprise.

Have a colour target and a drawing? Send both and we will quote against your own pass criteria.

Send a colour target

Ready when your drawing is

Send a STEP file, a sketch or a photo of the part that needs copying. You will have a manufacturability read and a firm number the next working day.

WeChat QR code Scan to chat